(Left) Voltage versus displacement; (Right) Displacement versus time |
|
"Squirming", a type of buckling with n = 1 circumferential wave. Squirming occurs when the axial stiffness is much smaller than the circumferential stiffness |
|
A locally failed (buckled) composite column under combined heat flux and compressive load |
|
Delamination, matrix cracking and fiber kinking in an axially compressed laminated composite |
|
Carbon fiber bundle kinking (buckling) under axial compression |
|
|
|
|
|
|
|
|
|
Fiber kinking in a laminated composite structure |
|
Buckled plate/wide column (Fig. 7); Load-end-shortening (Fig. 8); damage (Figs. 9,10; Load-deflection (Fig.11) |
|
Dynamic and sound radiation characteristics of rectangular thin plates with general boundary conditions |
|
Buckling of composite plate with edge stringers from residual thermal stresses caused by post-curing cooling of the axially stiffened plate |
|
Bone buckling and fracture: a biomechanics approach |
|
|
|
|
|
|
|
|
|
Angle of buckle nodal lines in an axially compressed long anisotropic [45deg.] plate |
|
Axial impact on cruciform structure: (left) test specimen; (right) finite element simulation |
|
Buckling of axially compressed stub, concrete-filled steel column |
|
Simulation of dynamic crushing of a box beam |
|
Thin-walled crushed square tube |
|
|